Sunday, May 25, 2014

Outboard impeller replacement

After you remove this grommet, you can unfasten the transmission linkage.
Our Mariner 5 hp was taken in on a trade last year.  It was spitting plenty of water so we used it for the season but now is the time to replace the impeller.  It is way better to replace it too early that too late.

We ordered the impeller, 2 extra shear pins and a cotter pin from Boats.net.
Here are photos and descriptions of the process:


Here we are removing the prop and unbolting the lower unit.

Here we are removing the impeller housing.
Here is the worn impeller.  Two fins were cracked
so we got it in the nick if time.
If it disintegrates while running, pieces can get lodged in passageways.


Here is the drive shaft assembly.
It is unrelated to the impeller, we just wanted to see it's condition.
Looks good.

This is the new shear pin.  The grooves make for weak spots that will fail if you hit a stump.
This can save the prop.  If you have pliers with you and a spare shear pin, you can keep boating.

Back in business!




SUP deck mold

We stripped the mold off the plug.
This afternoon we trimmed the rough edge and sanded it as well.
The mold looks great.  We will go over it with 1500 grit paper wet then re buff to get rid of the PVA texture.
We added a stringer in the mold on the centerline, but since the profile is thin it still has some flex in it.  We will place the mold back on top of the hull mold and add a rigid frame to it.
Here are some photos of the deck mold:




Saturday, May 24, 2014

Deck Mold: glass work

We added the layers of glass to the gel coated mold.
After the resin cured to the touch, we moved the whole shebang out to the mid-day sun.
UV light really speeds up the hard curing of resin.
We plan on stripping the mold off the deck plug tonight.

Curing with Mr. Sun.  The edge of the mold will get cut and sanded so it has a nice edge.

This photo shows the two half molds together.
The board will float in this trim, but 3 or 4 inches lower.

Thursday, May 22, 2014

Deck plug: ready to mold

After many passes of fairing and sanding the deck plug is ready to mold.
This process was about 10 times faster than the hull plug.  The two reasons for this are the hull is a bit more complicated and secondly, the clock is ticking.  Summer is almost here.  We have got to get this thing done.

The photo shows the plug waxed and coated in PVA.  In the morning, we will spray on the gelcoat and in the evening we will start adding glass to build up the mold.

We expect to start building boards next week.


This photo shows the deck plug on top of the hull mold.  You can get an idea of the board's profile from this angle.
It has a slight rocker and a piercing bow.  It will make a great touring board.

Saturday, May 17, 2014

SUP deck plug taking shape...

We have built up the plug for the deck of our new SUP.  We used foam an now Bondo.
It is getting close to the shape we are after.  There will be more sanding and fairing tomorrow, then we will start the gel coat layers.  Like on the hull plug, the gel coat will give us a surface we can bring up to a gloss.




Tuesday, May 13, 2014

Sea State 12 foot SUP: deck plug forming

We polished the mold and trimmed the edge of the mold.  But before casting parts we decided to start making the mold for the deck of this SUP.

To do this, we are building up the shape we want in rigid foam and spray foam.  This gets disk sanded to shape.  After we get the shape roughed in, we will cover the foam with glass cloth and epoxy.  We will gradually work the shape into a moldable plug.  Then we will create the mold and will have all we need to begin producing parts.

Here is today's work:

The deck plug being formed inside of the hull mold.
The flange is clearly visible and will provide space to form the deck mold flange.



Tools of the trade.  The pioneers would not be impressed.

A radius edge piece provides a fair line.

Thursday, May 8, 2014

SUP Plug: Step #12 New Mold !

We pulled off the mold today and it looks great.  Much glossier than our last years model.
I can't wait to form our first hull.
Here is a video of popping the mold off the plug:


Here is a close up video of the bow and interior surface before cleaning off the PVA.



Wednesday, May 7, 2014

SUP Plug: Steps 9, 10 and 11 !

After an thorough polishing, we waxed the plug 6 times and buffed it.
Next was a spray coating of PVA. This is Poly Vinyl Acetate.  This stuff forms a very thin film on a plug or mold and allows you to separate the new from the old.  For a large plug or mold, we spray it on with an automotive type paint air gun.  This dries quickly.  It is solvent proof but washes off after the processing with warm water.  After you pull a few parts from a mold, you can leave out the PVA and just use wax.
Next we used the cup gun to apply a layer of gel coat.  We just used regular tinted gel coat.  If we are happy with the shape and plan on making many hulls, we will make a second mold with tooling gel coat which has a harder surface.
Last night we did a wet layup of chopped strand mat fiberglass which was the first layer of glass on the mold.  Today we will add several more layers to make a stiff mold.

the plug after polishing and waxing

PVA (the parting film) and wax

This is the gel coated plug before we added fiberglass.
This coating will be the tooling surface of the working mold.

This photo shows the mold beginning to take shape.  This is the first layer of glass.

Tuesday, April 22, 2014

SUP Plug: Step #8

Taking it up to a polish.
After a bout of other work, I have been able to spend some time on the plug this week.
Our goal is to make a mold of the plug before Sunday.

This will be the first of at least two molds.
To get there, we need to sand up through the grits to about 1500 grit.
Yesterday, after a little more spot filling and sanding, we achieved the uniform shape we needed.
So today we gave the plug a even sanding with 120 grit paper then 220 paper.
Tomorrow we will do 320 grit dry then 320 grit wet.
Each finer pass we will do first dry then wet.
After we get to 1500 wet, we will use buffing compound and a wool pad to bring it up to a mirror finish.


Monday, April 7, 2014

Laser Trailer overhaul

Once we had everything off the trailer, prepping for paint is straight forward.  We used an orbital sander where we could and a wire brush where we had to.
We re-primed the frame and let it thoroughly dry.
We also took apart the wheel hubs, cleaned and re packed the bearings in good grease.
Next came spraying on a glossy black enamel paint.
While this was drying we worked on cutting the new bunk boards.

The bearings were dirty but still have plenty of life.

After a thorough cleaning we re-packed the bearings with marine grease.

Snug with no play, but not too tight!

With a leaf blower we flushed out a thousand acorns. 

Poor squirrel.


We scribed the bunks to the underside of the hull when it was upside down in the shop.  Then we used the big Silver band saw for the cuts.  After a coating of clear epoxy was applied, we used wide nylon strapping for the liners.
This was epoxied in place and the overhang was pulled down with brass tacks.

The Laser sits perfectly on it bunks in this position.  Now we just need to adjust the front bumper, add new lighting and wheels.

Thursday, April 3, 2014

While the Laser is off the trailer

While the Laser is getting a mani pedi we thought it was a great time to rejuvinate the trailer.
The paint was peeling and rust has crept around a bit.  The lights are shot and the wheels are dry rotted.

Last year when we got it, we gave the trailer a quick light sanding and sprayed on some primer to stop the deterioration.
Today once we got the lights and wires ripped off and the wooden bunk boards off we had a great opportunity to re-sand and prep for paint.

The rust is just on the surface so it is really an easy project.

A Laser trailer in need of help.


Rotted and rusty but the bearings are good.
The old bunk boards
The worn out electrics.

Stripped down and ready to sand.

Laser mani pedi

Now that the deck is gleaming white and the gel coat is hard, we wanted to address the hull bottom in the comfort of the shop.
We flipped it over on the horses and took care of a few items.
First was to remove the old State ID numbers.  They were peeling and not ours.
Next we filled in a few scratches in the hull with colored gel coat.  We didn't want to spend too much time on matching but the contrast is now not so glaring.
Then we got out the buffer and some compound and polished the hull.
Tomorrow we will instal the new self bailer and wax the hull.