Showing posts with label Making a SUP mold. Show all posts
Showing posts with label Making a SUP mold. Show all posts

Saturday, May 24, 2014

Deck Mold: glass work

We added the layers of glass to the gel coated mold.
After the resin cured to the touch, we moved the whole shebang out to the mid-day sun.
UV light really speeds up the hard curing of resin.
We plan on stripping the mold off the deck plug tonight.

Curing with Mr. Sun.  The edge of the mold will get cut and sanded so it has a nice edge.

This photo shows the two half molds together.
The board will float in this trim, but 3 or 4 inches lower.

Tuesday, May 13, 2014

Sea State 12 foot SUP: deck plug forming

We polished the mold and trimmed the edge of the mold.  But before casting parts we decided to start making the mold for the deck of this SUP.

To do this, we are building up the shape we want in rigid foam and spray foam.  This gets disk sanded to shape.  After we get the shape roughed in, we will cover the foam with glass cloth and epoxy.  We will gradually work the shape into a moldable plug.  Then we will create the mold and will have all we need to begin producing parts.

Here is today's work:

The deck plug being formed inside of the hull mold.
The flange is clearly visible and will provide space to form the deck mold flange.



Tools of the trade.  The pioneers would not be impressed.

A radius edge piece provides a fair line.

Wednesday, May 7, 2014

SUP Plug: Steps 9, 10 and 11 !

After an thorough polishing, we waxed the plug 6 times and buffed it.
Next was a spray coating of PVA. This is Poly Vinyl Acetate.  This stuff forms a very thin film on a plug or mold and allows you to separate the new from the old.  For a large plug or mold, we spray it on with an automotive type paint air gun.  This dries quickly.  It is solvent proof but washes off after the processing with warm water.  After you pull a few parts from a mold, you can leave out the PVA and just use wax.
Next we used the cup gun to apply a layer of gel coat.  We just used regular tinted gel coat.  If we are happy with the shape and plan on making many hulls, we will make a second mold with tooling gel coat which has a harder surface.
Last night we did a wet layup of chopped strand mat fiberglass which was the first layer of glass on the mold.  Today we will add several more layers to make a stiff mold.

the plug after polishing and waxing

PVA (the parting film) and wax

This is the gel coated plug before we added fiberglass.
This coating will be the tooling surface of the working mold.

This photo shows the mold beginning to take shape.  This is the first layer of glass.

Thursday, November 14, 2013

SUP Plug: Step #5 Gel-Coat

The SUP's plug is getting close to the uniform surface we are after.  But from experience we know there are problems that are hard to detect.  One thing that really helps is to spray on a layer of gel-coat.
By giving the surface a uniform color and material, the eye has a much better chance of spotting problems.
With this first layer of gel-coat, we will add a tint color.  Pure white is just too hard to see differences in.    
We also added a wax sanding aid to the gel-coat.  This allows the surface to cure hard so it is easier to sand.
After this layer hardens, we will continue sanding.  What else.

Here is white gel-coat in spay cup and a concentrated
blue tint color we add.

Here are the cup gun parts.
Mixed, assembled and ready to spray.

Thursday, October 31, 2013

SUP Plug forming: Step #2

 After the bow is pulled together, the hull bottom naturally forms a nice gentle v shape.
So now after the shape is secured, we have the heights or thickness of the board established.  The next thing to do is to set the sheer line or top edge of the entire deck surface.
I do this by ripping some 1/4 inch strips of wood (poplar).  I then mark out from the hull bottom 1 inch around the edge of the hull.

I do taper in to "0" at the bow and stern.  Next I shoot in the poplar strips to these markings.  This edge gives us something to fair to and hopefully keep the shape of the sides fair.

Next I fill in the void with foam.  I've used bondo and wood before, but foam is fast and it is only a base for further fairing.

Here you can see the poplar strip at the bottom edge of the sanded foam.

A couple of passes with great stuff, let it firm up then sand it down.

These two photos show the foam before and after disk sanding to the chine and shear line.


 Next I mark the center line with a string to make sure we are straight.  On this board I wanted a detail at the centerline to provide a little thickness for strength.  It will not be a skeg, just a slight rounded v.  The internal deck supports made of carbon fiber tube will rest on this centerline.
To form this, first we start with a furring strip.


The bow will have a pronounced v section and we form this by adding a vertical piece of wood. 
After the epoxy holding it sets, we mark a nice fair transition  and plane it down.


Then we sand it below the eventual
final surface.
Here foam is shot in to conserve
fairing compound.


Next we will start adding many passes of
fairing compound.

Monday, October 28, 2013

Shaping the next SUP in our line: Step #1

This weekend we started the process of forming a plug to make a mold to make out next line of SUPs.
The plan was to make some improvements that would allow us to make a hull that is more rigid, lighter and a little more graceful.

The new hull form is that of a flat water touring hull.  This is a displacement hull. This means a long form, low rocker and a water cutting bow. SUPs that are used in surf become planning hulls and benefit from rocker and being as short as practical.  All SUPs that are not being used this way (95 + %) are displacement hulls whether they are designed this way or not.

Our new board started out with these concepts in mind and this sketch:
From this start we began to loft the shape onto ply.
We have worked out a process to get to the plug.
Here it is...
We first get a ply material.  Of course, the plug never gets anywhere near water, so almost any ply will work.  In the past we have used masonite, this time we are using OSB.
We use battens to draw on a half profile.  This is one side of the board up to the centerline.
We use the machine edge of the ply for the center because it is reliably straight.
Once this is cut we use a hand planer to smooth the outer profile.  Then we use this shape to cut out it's other half.  These two halves are then affixed to the molding surface.

Because the length of the board is longer than standard sheet goods, we have to sister together the parts.  We do this by adding a ply piece on the underside with glue and screws.  This makes a stiff spot in the bendable ply but if it is in near the middle of the board this is not a problem and will be sanded and faired away.
This is the lap joint.
The next thing we do is to make a surface which mimics the shape of the eventual deck of the SUP.
We do this by bending an oversized piece of ply on saw horses.  The extra width provides a place for the flange of the mold.  The plug is formed right up to this plane and when the parts come out of the mold they have this same curved shape that will accept the deck.  Here some photos:
This is the sistered together half board profile.  It is  11 feet  9 inches.
Once the fairing is complete, the board will grow to an even 12 feet.

Here is the deck molding surface.  We introduced some rocker into this plane for fun and beauty.  The half shape is being affixed with specific heights and with a taper.


The thickness of the board is determined by this height.  We have set the maximum thickness of this SUP at 5 inches.
This shows the two halves set on the centerline.
A bit of material was removed on both sides in the rear.
They are screwed down flush at the tail and nowhere else yet.
When the bow is pulled together, this introduces a
little pucker which gives the hull a 'v' profile.
A sistered board underneath holds it together.
Then shims and screws are used to support this
shape.